Show simple item record

dc.contributor.authorSukanto, Heru
dc.contributor.authorBudiana, Eko Prasetya
dc.contributor.authorRaharjo, Wijang Wisnu
dc.date.accessioned2014-12-02T07:58:06Z
dc.date.available2014-12-02T07:58:06Z
dc.date.issued2014-12-04
dc.identifier.citation[1] Sahwan, F.L., Martono, D.H., Wahyono, S., Wiyosidharmo, L.A., 2005, SistemPengolahanLimbahPlastik di Indonesian, JurnalTeknologiLingkungan, Vol. 6 (1), pp. 311-318. [2] Aloma K.K., dkk., 2005, Pengaruh Anti OksidaTerhadapDegradasiPlastikPolipropilen, PuslitbangIptekBahan-BATAN, JurnalSainsMateri Indonesia, Vol 6-No.12, pp. 29-54. [3] Juma, M., Koren, Z., Markos, J., Annus, J., Jelemesky, L., 2006, Pyrolysis and Combustion of Scrap Tire, Petroleum & Coal, Vol. 48 (1), pp. 15-26. [4] ---, 1998, ASTM D 1435, standards, Standard Test Methode for Determining The Izod Impact Strength of Plastic, New York. [5] ---, 1998, ASTM D 790-97, standards, Standard Test Methode for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials, New York. [6] Popa, I.M,dkk, 2013, Mechanical Properties and Weathering Behavior of Polypropylene-Hemp Shives Composites, Journal of Chemistry, Hindawi Publishing Corporation, Vol. 2013, Artcicle ID 343068, pp 1-8. [7] Howarth, G.A, 2000, Legislation-compliant Polyurethane and Epoxy Coatings, Pigment & Resin Technology, Vol 29, pp 325-336. [8] Roylance, D., 1978, Weathering of Fiber-Reinforced Epoxy Composites, Polymer Engineering and Science, Vol. 18, No 4.en_US
dc.identifier.issn2407-4330
dc.identifier.urihttp://hdl.handle.net/11617/4960
dc.description.abstractThe recycled polypropylene (rPP) –rubber composite tends to depict the mechanical strength decreasing and physically degradation as well when installed as an outdoor application. The research investigated several materials which they can be applied as a protective coating materialsfor the composite. Oil based paint, waterproof paint, unsaturated polyester, and repoxy resins were selected materials to be examined.The raw materials of the composite were recycled rPP and tire after used in the powder state with mesh of 20 both. The composite consisted of rPP and rubber mixing with volume ratio of 7:3. Pressured sintering process was adopted for producing the composite with main parameters setting of temperature, pressure and holding time were 120 o C, 1 MPa and 5 minutes respectively. The coating materials were sprayed on the composite surface with the thickness could be neglected. The speciments were just layed on the special table during weather exposuring for three months continuously. The investigation included macro and SEM immages and bending test.The result reveals that the color degradation occured on the composite surface without coating after one month exposuring while cracks appear after exposuring takes time of two months and they tend to become propagated until the end of the third month. The SEM immages observation on fracture bending test showsthat the bonding between the plastic and the rubber began to be separated due to the influence of photo-degradation. The fracture are begun after the first month of weather exposuring. The waterproof coating provides the most stable of composite under bending test whereas unsaturated polyester coating has the highest bending strength overall exposuring periodesen_US
dc.publisherUniversitas Muhammadiyah Surakartaen_US
dc.subjectpolypropyleneen_US
dc.subjectcoatingen_US
dc.subjectexposure to weatheren_US
dc.subjectbending testen_US
dc.titleInvestigation Of Coating Materials On Recycled Polypropilene and Rubber Composite Under * Weather Exposureen_US